{"_buckets": {"deposit": "8fae14e8-010a-41bf-b34e-04020b717612"}, "_deposit": {"created_by": 3, "id": "4029", "owners": [3], "pid": {"revision_id": 0, "type": "depid", "value": "4029"}, "status": "published"}, "_oai": {"id": "oai:nitech.repo.nii.ac.jp:00004029", "sets": ["31"]}, "author_link": ["11735", "11733", "11734"], "item_10001_alternative_title_24": {"attribute_name": "その他(別言語等)のタイトル", "attribute_value_mlt": [{"subitem_alternative_title": "ZrOCl_2 ノウコウ ヨウセキ ノ スイネツ ショリ ニヨル ジルコニア キュウジョウ ギシュウ リュウシ ノ セイセイ"}, {"subitem_alternative_title": "Formation of Spherically Aggregated ZrO_2 Particles by Thermal Hydrolysis of ZrOCl_2 Concentrated Solution"}]}, "item_10001_biblio_info_28": {"attribute_name": "書誌情報", "attribute_value_mlt": [{"bibliographicIssueDates": {"bibliographicIssueDate": "1990-03-01", "bibliographicIssueDateType": "Issued"}, "bibliographicIssueNumber": "1135", "bibliographicPageEnd": "304", "bibliographicPageStart": "300", "bibliographicVolumeNumber": "98", "bibliographic_titles": [{"bibliographic_title": "Journal of the Ceramic Society of Japan"}]}]}, "item_10001_description_36": {"attribute_name": "内容記述", "attribute_value_mlt": [{"subitem_description": "Spherically aggregated ZrO_2 particles of about 1 μm with narrow size distribution were obtained by hydrothermal treatment of highly concentrated ZrOCl_2 solutions at 200℃ following the heat-treatment at 300℃ in air to dry. The aggregates are joined each other and are easily collapsed and dispersed to ultrafine particles of smaller than 10 nm by adding water before drying. The powder composed of the aggregates maintaining the shape as well as formed at the stage of the hydrothermal treatment was obtained when the \u0027double structured vessel\u0027 was employed for the hydrothermal treatment.", "subitem_description_type": "Other"}]}, "item_10001_description_38": {"attribute_name": "フォーマット", "attribute_value_mlt": [{"subitem_description": "application/pdf", "subitem_description_type": "Other"}]}, "item_10001_full_name_27": {"attribute_name": "著者別名", "attribute_value_mlt": [{"nameIdentifiers": [{"nameIdentifier": "11733", "nameIdentifierScheme": "WEKO"}], "names": [{"name": "Daimon, Keiji"}]}]}, "item_10001_publisher_29": {"attribute_name": "出版者", "attribute_value_mlt": [{"subitem_publisher": "The Ceramic Society of Japan"}]}, "item_10001_source_id_30": {"attribute_name": "ISSN", "attribute_value_mlt": [{"subitem_source_identifier": "09145400", "subitem_source_identifier_type": "ISSN"}]}, "item_10001_source_id_32": {"attribute_name": "書誌レコードID(NCID)", "attribute_value_mlt": [{"subitem_source_identifier": "AN10040326", "subitem_source_identifier_type": "NCID"}]}, "item_10001_version_type_33": {"attribute_name": "著者版フラグ", "attribute_value_mlt": [{"subitem_version_resource": "http://purl.org/coar/version/c_970fb48d4fbd8a85", "subitem_version_type": "VoR"}]}, "item_creator": {"attribute_name": "著者", "attribute_type": "creator", "attribute_value_mlt": [{"creatorNames": [{"creatorName": "大門, 啓志"}, {"creatorName": "ダイモン, ケイジ", "creatorNameLang": "ja-Kana"}], "nameIdentifiers": [{"nameIdentifier": "11733", "nameIdentifierScheme": "WEKO"}]}, {"creatorNames": [{"creatorName": "山田, 淳二"}], "nameIdentifiers": [{"nameIdentifier": "11734", "nameIdentifierScheme": "WEKO"}]}, {"creatorNames": [{"creatorName": "加藤, 悦朗"}], "nameIdentifiers": [{"nameIdentifier": "11735", "nameIdentifierScheme": "WEKO"}]}]}, "item_files": {"attribute_name": "ファイル情報", "attribute_type": "file", "attribute_value_mlt": [{"accessrole": "open_date", "date": [{"dateType": "Available", "dateValue": "2017-01-23"}], "displaytype": "detail", "download_preview_message": "", "file_order": 0, "filename": "JCSJ 98_300.pdf", "filesize": [{"value": "3.1 MB"}], "format": "application/pdf", "future_date_message": "", "is_thumbnail": false, "licensefree": "(c) 1990 The Ceramic Society of Japan", "licensetype": "license_free", "mimetype": "application/pdf", "size": 3100000.0, "url": {"label": "本文_fulltext", "url": "https://nitech.repo.nii.ac.jp/record/4029/files/JCSJ 98_300.pdf"}, "version_id": "e1b9a6d6-3281-4aca-b7de-14218756ee0c"}]}, "item_language": {"attribute_name": "言語", "attribute_value_mlt": [{"subitem_language": "jpn"}]}, "item_resource_type": {"attribute_name": "資源タイプ", "attribute_value_mlt": [{"resourcetype": "journal article", "resourceuri": "http://purl.org/coar/resource_type/c_6501"}]}, "item_title": "ZrOCl_2濃厚溶液の水熱処理によるジルコニア球状凝集粒子の生成", "item_titles": {"attribute_name": "タイトル", "attribute_value_mlt": [{"subitem_title": "ZrOCl_2濃厚溶液の水熱処理によるジルコニア球状凝集粒子の生成"}]}, "item_type_id": "10001", "owner": "3", "path": ["31"], "permalink_uri": "https://nitech.repo.nii.ac.jp/records/4029", "pubdate": {"attribute_name": "公開日", "attribute_value": "2012-11-06"}, "publish_date": "2012-11-06", "publish_status": "0", "recid": "4029", "relation": {}, "relation_version_is_last": true, "title": ["ZrOCl_2濃厚溶液の水熱処理によるジルコニア球状凝集粒子の生成"], "weko_shared_id": -1}
ZrOCl_2濃厚溶液の水熱処理によるジルコニア球状凝集粒子の生成
https://nitech.repo.nii.ac.jp/records/4029
https://nitech.repo.nii.ac.jp/records/4029d044e918-cc07-4664-a259-8b7105e0d4f0
名前 / ファイル | ライセンス | アクション |
---|---|---|
本文_fulltext (3.1 MB)
|
(c) 1990 The Ceramic Society of Japan
|
Item type | 学術雑誌論文 / Journal Article(1) | |||||
---|---|---|---|---|---|---|
公開日 | 2012-11-06 | |||||
タイトル | ||||||
タイトル | ZrOCl_2濃厚溶液の水熱処理によるジルコニア球状凝集粒子の生成 | |||||
言語 | ||||||
言語 | jpn | |||||
資源タイプ | ||||||
資源タイプ識別子 | http://purl.org/coar/resource_type/c_6501 | |||||
資源タイプ | journal article | |||||
その他(別言語等)のタイトル | ||||||
その他のタイトル | ZrOCl_2 ノウコウ ヨウセキ ノ スイネツ ショリ ニヨル ジルコニア キュウジョウ ギシュウ リュウシ ノ セイセイ | |||||
その他(別言語等)のタイトル | ||||||
その他のタイトル | Formation of Spherically Aggregated ZrO_2 Particles by Thermal Hydrolysis of ZrOCl_2 Concentrated Solution | |||||
著者 |
大門, 啓志
× 大門, 啓志× 山田, 淳二× 加藤, 悦朗 |
|||||
著者別名 | ||||||
姓名 | Daimon, Keiji | |||||
書誌情報 |
Journal of the Ceramic Society of Japan 巻 98, 号 1135, p. 300-304, 発行日 1990-03-01 |
|||||
出版者 | ||||||
出版者 | The Ceramic Society of Japan | |||||
ISSN | ||||||
収録物識別子タイプ | ISSN | |||||
収録物識別子 | 09145400 | |||||
書誌レコードID(NCID) | ||||||
収録物識別子タイプ | NCID | |||||
収録物識別子 | AN10040326 | |||||
著者版フラグ | ||||||
出版タイプ | VoR | |||||
出版タイプResource | http://purl.org/coar/version/c_970fb48d4fbd8a85 | |||||
内容記述 | ||||||
内容記述タイプ | Other | |||||
内容記述 | Spherically aggregated ZrO_2 particles of about 1 μm with narrow size distribution were obtained by hydrothermal treatment of highly concentrated ZrOCl_2 solutions at 200℃ following the heat-treatment at 300℃ in air to dry. The aggregates are joined each other and are easily collapsed and dispersed to ultrafine particles of smaller than 10 nm by adding water before drying. The powder composed of the aggregates maintaining the shape as well as formed at the stage of the hydrothermal treatment was obtained when the 'double structured vessel' was employed for the hydrothermal treatment. | |||||