{"_buckets": {"deposit": "042fc5ea-95c2-4a93-978c-e0fa6fda0fb5"}, "_deposit": {"created_by": 3, "id": "4199", "owners": [3], "pid": {"revision_id": 0, "type": "depid", "value": "4199"}, "status": "published"}, "_oai": {"id": "oai:nitech.repo.nii.ac.jp:00004199", "sets": ["31"]}, "author_link": ["12523", "8759", "12521", "12524"], "item_10001_alternative_title_24": {"attribute_name": "その他(別言語等)のタイトル", "attribute_value_mlt": [{"subitem_alternative_title": "サンカ ヒマク デ ヒフク サレタ ヒケッショウ SiC ケイ センイ ノ ネツ アンテイセイ"}, {"subitem_alternative_title": "Thermal Stability of Amorphous SiC Fiber Coated with Oxide Film"}]}, "item_10001_biblio_info_28": {"attribute_name": "書誌情報", "attribute_value_mlt": [{"bibliographicIssueDates": {"bibliographicIssueDate": "1993-02-01", "bibliographicIssueDateType": "Issued"}, "bibliographicIssueNumber": "1170", "bibliographicPageEnd": "210", "bibliographicPageStart": "204", "bibliographicVolumeNumber": "101", "bibliographic_titles": [{"bibliographic_title": "Journal of the Ceramic Society of Japan"}]}]}, "item_10001_description_36": {"attribute_name": "内容記述", "attribute_value_mlt": [{"subitem_description": "Using Tyranno fiber containing 13% O (T-2), suppression of pyrolysis with oxide film was investigated at temperatures from 1573 to 1773K. The gas stream was changed to Ar, immediately after an oxide film of a given thickness was formed on the fiber in O2. At temperatures lower than 1723K, the pyrolysis was suppressed. The core fiber crystallized slightly, and the oxide film changed from amorphous silica into cristobalite. The tensile strength was 1.26 to 1.45GPa when treated at 1723K. At 1773K, the oxide film disappeared, and the core fiber decomposed completely to β-SiC. The resulting fiber was too weak to measure the strength. These results were compared with those obtained in Tyranno fiber containing 18% O (T-1) and Nicalon fiber (NL200).", "subitem_description_type": "Other"}]}, "item_10001_description_38": {"attribute_name": "フォーマット", "attribute_value_mlt": [{"subitem_description": "application/pdf", "subitem_description_type": "Other"}]}, "item_10001_full_name_27": {"attribute_name": "著者別名", "attribute_value_mlt": [{"nameIdentifiers": [{"nameIdentifier": "8759", "nameIdentifierScheme": "WEKO"}, {"nameIdentifier": "1000040335089", "nameIdentifierScheme": "NRID", "nameIdentifierURI": "http://rns.nii.ac.jp/nr/1000040335089"}], "names": [{"name": "Kakimoto, Ken-ichi"}]}]}, "item_10001_publisher_29": {"attribute_name": "出版者", "attribute_value_mlt": [{"subitem_publisher": "The Ceramic Society of Japan"}]}, "item_10001_source_id_30": {"attribute_name": "ISSN", "attribute_value_mlt": [{"subitem_source_identifier": "09145400", "subitem_source_identifier_type": "ISSN"}]}, "item_10001_source_id_32": {"attribute_name": "書誌レコードID(NCID)", "attribute_value_mlt": [{"subitem_source_identifier": "AN10040326", "subitem_source_identifier_type": "NCID"}]}, "item_10001_version_type_33": {"attribute_name": "著者版フラグ", "attribute_value_mlt": [{"subitem_version_resource": "http://purl.org/coar/version/c_970fb48d4fbd8a85", "subitem_version_type": "VoR"}]}, "item_creator": {"attribute_name": "著者", "attribute_type": "creator", "attribute_value_mlt": [{"creatorNames": [{"creatorName": "下尾, 聰夫"}, {"creatorName": "\u0026EMPTY\u0026", "creatorNameLang": "ja-Kana"}], "nameIdentifiers": [{"nameIdentifier": "12521", "nameIdentifierScheme": "WEKO"}]}, {"creatorNames": [{"creatorName": "柿本, 健一"}, {"creatorName": "カキモト, ケンイチ", "creatorNameLang": "ja-Kana"}], "nameIdentifiers": [{"nameIdentifier": "8759", "nameIdentifierScheme": "WEKO"}, {"nameIdentifier": "1000040335089", "nameIdentifierScheme": "NRID", "nameIdentifierURI": "http://rns.nii.ac.jp/nr/1000040335089"}]}, {"creatorNames": [{"creatorName": "陳和, 民"}], "nameIdentifiers": [{"nameIdentifier": "12523", "nameIdentifierScheme": "WEKO"}]}, {"creatorNames": [{"creatorName": "岡村, 清人"}], "nameIdentifiers": [{"nameIdentifier": "12524", "nameIdentifierScheme": "WEKO"}]}]}, "item_files": {"attribute_name": "ファイル情報", "attribute_type": "file", "attribute_value_mlt": [{"accessrole": "open_date", "date": [{"dateType": "Available", "dateValue": "2017-01-23"}], "displaytype": "detail", "download_preview_message": "", "file_order": 0, "filename": "JCSJ 101_204.pdf", "filesize": [{"value": "3.0 MB"}], "format": "application/pdf", "future_date_message": "", "is_thumbnail": false, "licensefree": "(c) 1993 The Ceramic Society of Japan", "licensetype": "license_free", "mimetype": "application/pdf", "size": 3000000.0, "url": {"label": "本文_fulltext", "url": "https://nitech.repo.nii.ac.jp/record/4199/files/JCSJ 101_204.pdf"}, "version_id": "afe0391a-c3ec-4a71-b77b-2838327b2a11"}]}, "item_language": {"attribute_name": "言語", "attribute_value_mlt": [{"subitem_language": "jpn"}]}, "item_resource_type": {"attribute_name": "資源タイプ", "attribute_value_mlt": [{"resourcetype": "journal article", "resourceuri": "http://purl.org/coar/resource_type/c_6501"}]}, "item_title": "酸化皮膜で被覆された非晶質 SiC 系繊維の熱安定性", "item_titles": {"attribute_name": "タイトル", "attribute_value_mlt": [{"subitem_title": "酸化皮膜で被覆された非晶質 SiC 系繊維の熱安定性"}]}, "item_type_id": "10001", "owner": "3", "path": ["31"], "permalink_uri": "https://nitech.repo.nii.ac.jp/records/4199", "pubdate": {"attribute_name": "公開日", "attribute_value": "2012-11-06"}, "publish_date": "2012-11-06", "publish_status": "0", "recid": "4199", "relation": {}, "relation_version_is_last": true, "title": ["酸化皮膜で被覆された非晶質 SiC 系繊維の熱安定性"], "weko_shared_id": 3}
酸化皮膜で被覆された非晶質 SiC 系繊維の熱安定性
https://nitech.repo.nii.ac.jp/records/4199
https://nitech.repo.nii.ac.jp/records/41990492064d-5c2e-438a-8198-fc7867151f04
名前 / ファイル | ライセンス | アクション |
---|---|---|
本文_fulltext (3.0 MB)
|
(c) 1993 The Ceramic Society of Japan
|
Item type | 学術雑誌論文 / Journal Article(1) | |||||
---|---|---|---|---|---|---|
公開日 | 2012-11-06 | |||||
タイトル | ||||||
タイトル | 酸化皮膜で被覆された非晶質 SiC 系繊維の熱安定性 | |||||
言語 | ||||||
言語 | jpn | |||||
資源タイプ | ||||||
資源タイプ識別子 | http://purl.org/coar/resource_type/c_6501 | |||||
資源タイプ | journal article | |||||
その他(別言語等)のタイトル | ||||||
その他のタイトル | サンカ ヒマク デ ヒフク サレタ ヒケッショウ SiC ケイ センイ ノ ネツ アンテイセイ | |||||
その他(別言語等)のタイトル | ||||||
その他のタイトル | Thermal Stability of Amorphous SiC Fiber Coated with Oxide Film | |||||
著者 |
下尾, 聰夫
× 下尾, 聰夫× 柿本, 健一× 陳和, 民× 岡村, 清人 |
|||||
著者別名 | ||||||
姓名 | Kakimoto, Ken-ichi | |||||
書誌情報 |
Journal of the Ceramic Society of Japan 巻 101, 号 1170, p. 204-210, 発行日 1993-02-01 |
|||||
出版者 | ||||||
出版者 | The Ceramic Society of Japan | |||||
ISSN | ||||||
収録物識別子タイプ | ISSN | |||||
収録物識別子 | 09145400 | |||||
書誌レコードID(NCID) | ||||||
収録物識別子タイプ | NCID | |||||
収録物識別子 | AN10040326 | |||||
著者版フラグ | ||||||
出版タイプ | VoR | |||||
出版タイプResource | http://purl.org/coar/version/c_970fb48d4fbd8a85 | |||||
内容記述 | ||||||
内容記述タイプ | Other | |||||
内容記述 | Using Tyranno fiber containing 13% O (T-2), suppression of pyrolysis with oxide film was investigated at temperatures from 1573 to 1773K. The gas stream was changed to Ar, immediately after an oxide film of a given thickness was formed on the fiber in O2. At temperatures lower than 1723K, the pyrolysis was suppressed. The core fiber crystallized slightly, and the oxide film changed from amorphous silica into cristobalite. The tensile strength was 1.26 to 1.45GPa when treated at 1723K. At 1773K, the oxide film disappeared, and the core fiber decomposed completely to β-SiC. The resulting fiber was too weak to measure the strength. These results were compared with those obtained in Tyranno fiber containing 18% O (T-1) and Nicalon fiber (NL200). | |||||