@article{oai:nitech.repo.nii.ac.jp:00004343, author = {太田, 敏孝 and 松原, 長 and 高橋, 実 and 引地, 康夫 and 鈴木, 久男}, issue = {1197}, journal = {Journal of the Ceramic Society of Japan}, month = {May}, note = {High-thermal-expansion ceramics consisting of nepheline (NaAlSiO_4) and leucite (KAlSi_2O_6) were prepared by sintering mixture of their powders. The ceramics obtained had the relative density of 70 to 90%, bending strength of 60 to 100 MPa and linear thermal expansion coefficient of 15×10^<-6>/℃ to 28×10^<-6>/℃ from room temperature to 600℃. The thermal expansion coefficient of the ceramics increased with increasing leucite content., application/pdf}, pages = {523--524}, title = {ネフェリン-リューサイト複合焼結体の熱膨張}, volume = {103}, year = {1995}, yomi = {オオタ, トシタカ} }